HRN EN 12390-8:2009
Ispitivanje očvrsnuloga betona -- 8. dio: Dubina prodora vode pod tlakom (EN 12390-8:2009)
Oznaka: | HRN EN 12390-8:2009 |
Naslov (HR): | Ispitivanje očvrsnuloga betona -- 8. dio: Dubina prodora vode pod tlakom (EN 12390-8:2009) |
Naslov (EN): | Testing hardened concrete -- Part 8: Depth of penetration of water under pressure (EN 12390-8:2009) |
Područje primjene (EN): | This European Standard specifies a method for determining the depth of penetration of water under pressure in hardened concrete which has been water cured. |
Izdanje: | 2 |
ICS: | 91.100.30 Beton i betonski proizvodi |
Tehnički odbor/pododbor: | TO 71, Beton |
Oznaka faze: | 95.99 - povlačenje HRN |
Glasilo (rasprava): | 2/2009 () |
Glasilo (objava): | 3/2009 () |
Glasilo (povlačenje): | 9/2019 () |
Način prihvaćanja: | pr - prihvaćanje strane norme u izvorniku |
Cijena #1: | Cijena: 20,00 € | Jezik: en | Cjenovni razred: B | Broj stranica: 8 |
Izvornik: | EN 12390-8:2009 |
Zamjenjuje: | HRN EN 12390-8:2001 |
Zamjenjena s: | HRN EN 12390-8:2019 |