HRN EN 12504-1:2009
Ispitivanje betona u konstrukcijama -- 1. dio: Izvađeni ispitni uzorci -- Uzimanje, pregled i ispitivanje tlačne čvrstoće (EN 12504-1:2009)
Oznaka: | HRN EN 12504-1:2009 |
Naslov (HR): | Ispitivanje betona u konstrukcijama -- 1. dio: Izvađeni ispitni uzorci -- Uzimanje, pregled i ispitivanje tlačne čvrstoće (EN 12504-1:2009) |
Naslov (EN): | Testing concrete in structures -- Part 1: Cored specimens -- Taking, examining and testing in compression (EN 12504-1:2009) |
Područje primjene (EN): | This European Standard specifies a method for taking cores from hardened concrete, their examination, preparation for testing and determination of compressive strength. NOTE 1 This European Standard does not give guidance on the decision to drill cores or on the locations for drilling. NOTE 2 This European Standard does not provide procedures for interpreting the core strength results. NOTE 3 For the assessment of in-situ compressive strength in structures and precast concrete components EN 13791 may be used. |
Izdanje: | 2 |
ICS: | 91.100.30 Beton i betonski proizvodi |
Tehnički odbor/pododbor: | TO 71, Beton |
Oznaka faze: | 95.99 - povlačenje HRN |
Glasilo (rasprava): | 2/2009 () |
Glasilo (objava): | 3/2009 () |
Glasilo (povlačenje): | 9/2019 () |
Način prihvaćanja: | pr - prihvaćanje strane norme u izvorniku |
Cijena #1: | Cijena: 25,00 € | Jezik: en | Cjenovni razred: C | Broj stranica: 11 |
Izvornik: | EN 12504-1:2009 |
Zamjenjuje: | HRN EN 12504-1:2000 |
Zamjenjena s: | HRN EN 12504-1:2019 |
Obrazac za naručivanje normativnih dokumenata i/ili publikacija (obrazac ob.025-2):